Possible improvements on Descender

One design flaw on Simple/Stop could be adressed: the locking flap.
I had both breaking rivits and small stones/mud getting into the slot of the flap or between the coild of the spring making it inoperable.

Some design ideas could be taken from carabiners. An open wire spring lock would be my start.
 
As a master tool and die maker I have some options which are not realistic for serial production, but from experience I could say that bobbins made from hardend stainless steel (1.4021) with an aluminium core and carbide sprayed aluminium bobbins are far superior, but unrealistic for a commercial product.
Bobbins made from mild stainless steel are cheap and heavy, that's all.

Never tested aluminium-bronze or beryllium-copper alloys, these might be even superior...but unrealistic.

As titanium (Ti) was mentioned...well, it's a hype. Even more solphisticted Ti alloys have pretty bad wear characteristics and bad heat conduction. Nothing you want to make a bobbin off.
Also a master toolmaker I used nitriding, also called nitriding, to harden the mild steel pillars and cam on a descender I designed and produced in the late 80's. and early 90's called the Jlock or Gemlok. Nitriding treatment is none distorting so the cams and pillars could be pre-drilled and tapped. The process lends itself to batch production and was quite cheap. The process can be applied to other low alloy metals. If I had continued production ( PPE reared it's ugly head and was very expensive for a sole trader) I would have tried aluminium for cams which I believe is a newer nitriding development. On mild steel as well as a corrosion resist finish the surface hardness was around 58 RC. Deeper and harder values can be reached depending on the nitiding process and base material used.
 
Back